(519) 307-1330Monday to Friday, 8 am to 5 pm ETEmergency service (905) 818-9397
Call

Cryogenic, thermal and media deflashing compared

Three ways to remove flash from moulded parts, and when plastic-media blasting is the one to pick.

By Surface Technologies engineering · Updated November 27, 2026 · 2 min read

Cryogenic deflashing

Parts are chilled with liquid nitrogen until the flash is brittle, then tumbled with polycarbonate media. Works well on rubber and soft thermoplastics; the running cost is nitrogen, and thin thermoset sections can crack.

Thermal deflashing

A controlled flame or gas ignition burns flash off. Common for some rubber and thermoplastic parts; unsuitable for thermosets and anything with a surface finish to protect.

Plastic-media (abrasive) deflashing

Room-temperature plastic media thrown by a wheel or air nozzle snaps brittle thermoset flash off without etching the part. No nitrogen, no heat, no warping, and the media recycles through the machine.

Choosing

Rubber and soft elastomers often favour cryogenic. Thermosets (BMC, phenolic, epoxy, DAP), electrical insulators and precision housings favour plastic media. Many moulders run both: a tumble machine for volume and an indexer for the fragile parts.

Automation

All four of our deflash models accept loaders, unloaders and robotic handling, so an automated deflashing cell can run with the operator doing something else.

Which materials suit which process

Rubber and soft thermoplastic elastomers must be frozen to make the flash brittle, so they are cryogenic work. Cured thermosets are brittle already and deflash at room temperature. Die-cast metals are a different problem again and are deburred with metallic or mineral media.

Operating cost

Cryogenic machines consume liquid nitrogen on every cycle, and that cost continues for the life of the machine. Room-temperature media deflashing has no cryogen cost; its consumables are plastic media and wear parts.

Effect on the part

Deep cooling can stress some parts and may cause condensation as they warm. Thermal deflashing, which burns flash off in a flash of combustion, is fast for internal burrs but is not suited to most moulded thermoset work. Plastic media at room temperature leaves dimensions and surface finish unchanged when the cycle is set correctly.

Questions to settle before choosing

What is the material? Can parts touch each other? How thick is the worst flash, and where is it? What volume runs per shift, and is flow continuous or in batches? What cleanliness does assembly need? The answers point to the process and then to the machine.

Tell us about the part

Send a drawing, a photo or the part details. We recommend the machine that fits and quote it.

Machine down? Emergency service (905) 818-9397

Call (519) 307-1330Request a quote